This forum will give you access to participate in discussions and attain resources via our vibrant waterjet community . This discussion board is intended for any waterjet user but the majority of the moderators are associates of Flow International Corporation. We will attempt to make this community an unbiased source of information regarding general waterjet topic areas. If you are a registered Flow Waterjet customer and require in-depth product support, please visit FlowParts.com.

Members Login
Username 
 
Password 
    Remember Me  
Post Info TOPIC: thin stainless sheet


Member

Status: Offline
Posts: 8
Date:
thin stainless sheet
Permalink  
 


hi , how does everyone handle cutting thin stainless sheets, im having problems with sheet bowing as i cut , goes from nozzle to far away and bad cut quality to touching and clogging nozzle.

 

thanks

r brintle

 



__________________
rsb


Member

Status: Offline
Posts: 20
Date:
Permalink  
 

This is a problem with any thin material as you will need to chase the head around with various weights and such. Putting more blades in helps but then it also creates more ares for the jet to deflect back up into the bottom of the material. We typically use foam insulation 1-1/2" thick when cutting this type of materials, it really helps prevent bottom damage. We use spent carbide blocks for weights and we generally wrap them in duct tape to prevent scratching. It takes a little busy work and knowing where the head will be going next to position the blocks properly to prevent any collisions with the nozzles. There are a couple companies that offer a whisker biscuit type cone that goes on over the nozzle to help decrease splash back and material buckle and they work somewhat but I dont like them due to not being able to see the nozzle tip standoff. If the tolerance allows you could also try cutting mutiple sheets deep. One other thing I have found that works well to minimize heat distortion is to hook a water hoze up near the nozzle, this keeps the piercing from developing alot of heat and keeps the material from buckling especially heat sensitive materials like aluminum.

 

Good luck

~GC~



__________________


Veteran Member

Status: Offline
Posts: 94
Date:
Permalink  
 

You can get some sheet metal screws and screw it down onto some luan or 1/4" plywood. It will hold it more firm and won't make as much of a mess as the foam.

__________________
Do not waste today regretting yesterday.
Page 1 of 1  sorted by
 
Quick Reply

Please log in to post quick replies.

Please note, the views and recommendations expressed by employees of Flow or it's partners on this website do not necessarily represent those of Flow International Corporation. For more information on this site's Terms of Use , please visit the DXF Copyright and Community Guidelines pages.

Important: Do not upload any DXF's or images without permission unless they consist entirely of content you or your company created.

By clicking "Upload file", you are representing that this DXF or image does not violate the WaterjetGroup.com's forum's Terms of Use and that you own all copyrights to this file or have authorization to upload it.