Welcome to the ultimate waterjet forum, WaterjetGroup.com!
This forum will give you access to participate in discussions and attain resources via our vibrant waterjet community . This discussion board is intended for any waterjet user but the majority of the moderators are associates of Flow International Corporation. We will attempt to make this community an unbiased source of information regarding general waterjet topic areas. If you are a registered Flow Waterjet customer and require in-depth product support, please visit FlowParts.com. font>
We cut a good quantity of various types of rubber, and have not found a way to completely eliminate the burr (well, maybe 'fuzz' is a better description) on the backside of the cut.
The cut quality itself is quite good, however.
Best results come from using a .007" water only orifice at 30ksi, as it seems a smaller stream correlates to less fuzz.
But we've found orifices less than .007 don't last, and even the .007s blow out when we try to crank up the pressure to 40-45ksi (so we can go faster).
I find that cutting many types of rubbers or plastics you get this type of a "burr". Most of the time you can run your finger down the side and it just comes off but overall I would say its just nature of the beast. Your orifice blowing out sounds like a seperate problem, i use diamonds (.003 - .007) for most of my water cuts and get hundreds of hours out of them.
This may not be practical but I have actually had luck eliminating the burr by freezing some rubber and plastics. Also, if it is possible to stack the material that will usually eliminate the burr on all layers except for the last. Even the last one will be better though.
We do have good luck stacking the parts we can, however, many of them are formed 3D parts which we cannot stack. And you're right, the burr can be removed with your fingernail, and we bought some small clay working knives to do it. Just a pain is all.
We've had terrible luck with diamond orifices (orifii?) on our abrasive head, so all we use are sapphires.... which seem to work well, averaging 30-50 hours per. We concluded that since we change from abrasive to water-only cutting head sometimes daily, the sapphires were much less sensitive to tightening torque than the diamonds.
Topend1, what sort of torque are you using for your water-only orifice nozzle nut?
I would agree with you, the diamonds are more sensitive (in my opinion) to the torque. As a heads up, Flow has some things coming out that will drastically improve orifice life across the board (shhhhh!).
Next time you buy a freezer, let me know so I can send you a big teal sticker....you can tell all your friends (who probably wouldn't give a darn) that you bought a Flow Freezer!
Please note, the views and recommendations expressed by employees of Flow or it's partners on this website do not necessarily represent those of Flow International Corporation. For more information on this site's Terms of Use , please visit the DXF Copyright and Community Guidelines pages.
Important: Do not upload any DXF's or images without permission unless they consist entirely of content you or your company created.
By clicking "Upload file", you are representing that this DXF or image does not violate the WaterjetGroup.com's forum's Terms of Use and that you own all copyrights to this file or have authorization to upload it.